In the Brinell testing method, the load should be pressed for a minimum of ____________

In the Brinell testing method, the load should be pressed for a minimum of ____________ Correct Answer 10 seconds

In the Brinell testing method, the test specimen is indented with a ball made of steel, with a diameter or 10 mm for a certain amount of time. The minimum time period is 10 seconds before the load is released.