In full annealing, the hypo eutectoid steel is heated from 30°C to 50°C above the upper critical temperature and then cooled
In full annealing, the hypo eutectoid steel is heated from 30°C to 50°C above the upper critical temperature and then cooled Correct Answer Slowly in the furnace
In full annealing, the hypo eutectoid steel is heated from 30°C to 50°C above the upper critical temperature and then cooled Slowly in the furnace