Eddy current inspection (ECI) is generally restricted to a depth below ___________
Eddy current inspection (ECI) is generally restricted to a depth below ___________ Correct Answer 6mm
Eddy current inspection is generally restricted to a depth below 6mm, It is because of the secondary induced current in the material and it also called as skin effect.